Description

To the comparable DIN-mark Pb99,94, mat. No 2.3030, acc. to DIN 1719 : 1986-01 applies: This slag-lead (soft lead) material is used as initial material for production of alloys and semi-finished products.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

11.34 g/cm³

Show Material materials with Density of 11.34 g/cm³

Typical for Pure/Low Alloyed Lead

Mechanical

PropertyTemperatureValueComment

Poisson's ratio

23.0 °C

0.4 [-]

Show Material materials with Poisson's ratio of 0.4 [-]

Typical for Pure/Low Alloyed Lead

Thermal

PropertyTemperatureValueComment

Melting point

327 °C

Show Material materials with Melting point of 327 °C

Typical for Pure/Low Alloyed Lead

Specific heat capacity

23.0 °C

112 - 134 J/(kg·K)

Show Material materials with Specific heat capacity of 112 - 134 J/(kg·K)

Typical for Pure/Low Alloyed Lead

Thermal conductivity

23.0 °C

34 - 35 W/(m·K)

Show Material materials with Thermal conductivity of 34 - 35 W/(m·K)

Typical for Pure/Low Alloyed Lead

Chemical properties

PropertyValue

Antimony

1E-3 %

Show Material materials with Antimony of 1E-3 %

Arsenic

1E-3 %

Show Material materials with Arsenic of 1E-3 %

Bismuth

0.01 %

Show Material materials with Bismuth of 0.01 %

Copper

1E-3 %

Show Material materials with Copper of 1E-3 %

Lead

99.99 %

Show Material materials with Lead of 99.99 %

Silver

2E-3 %

Show Material materials with Silver of 2E-3 %

Tin

1E-3 %

Show Material materials with Tin of 1E-3 %