General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 11.34 g/cm³ Show Material materials with Density of 11.34 g/cm³ | Typical for Pure/Low Alloyed Lead |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Poisson's ratio | 23.0 °C | 0.4 [-] Show Material materials with Poisson's ratio of 0.4 [-] | Typical for Pure/Low Alloyed Lead |
Tensile strength | 20.0 °C | 15 - 30 MPa Show Material materials with Tensile strength of 15 - 30 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Melting point | 327 °C Show Material materials with Melting point of 327 °C | Typical for Pure/Low Alloyed Lead | |
Specific heat capacity | 23.0 °C | 112 - 134 J/(kg·K) Show Material materials with Specific heat capacity of 112 - 134 J/(kg·K) | Typical for Pure/Low Alloyed Lead |
Thermal conductivity | 23.0 °C | 34 - 35 W/(m·K) Show Material materials with Thermal conductivity of 34 - 35 W/(m·K) | Typical for Pure/Low Alloyed Lead |
Chemical properties
Property | Value |
---|---|
Antimony | 0.2 - 0.3 % Show Material materials with Antimony of 0.2 - 0.3 % |
Lead | 99.7 % Show Material materials with Lead of 99.7 % |