General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 9.6 g/cm³ Show Material materials with Density of 9.6 g/cm³ | Typical for Lead Antimony |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Melting point | 235 - 305 °C Show Material materials with Melting point of 235 - 305 °C | Typical for Lead Antimony | |
Specific heat capacity | 23.0 °C | 130 - 159 J/(kg·K) Show Material materials with Specific heat capacity of 130 - 159 J/(kg·K) | Typical for Lead Antimony |
Thermal conductivity | 23.0 °C | 24 - 34 W/(m·K) Show Material materials with Thermal conductivity of 24 - 34 W/(m·K) | Typical for Lead Antimony |
Chemical properties
Property | Value |
---|---|
Antimony | 3.5 - 4.5 % Show Material materials with Antimony of 3.5 - 4.5 % |
Lead | 95.5 % Show Material materials with Lead of 95.5 % |