DIN 17640-1 Grade PbSb12

Want to keep this datasheet? Save it now in your required format

Description

The antimony-lead alloy (hard lead) PbSb12 is applicated as base alloy for production of alloys.

Related Standards

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

9.6 g/cm³

Show Material materials with Density of 9.6 g/cm³

Typical for Lead Antimony

Thermal

PropertyTemperatureValueComment

Melting point

235 - 305 °C

Show Material materials with Melting point of 235 - 305 °C

Typical for Lead Antimony

Specific heat capacity

23.0 °C

130 - 159 J/(kg·K)

Show Material materials with Specific heat capacity of 130 - 159 J/(kg·K)

Typical for Lead Antimony

Thermal conductivity

23.0 °C

24 - 34 W/(m·K)

Show Material materials with Thermal conductivity of 24 - 34 W/(m·K)

Typical for Lead Antimony

Chemical properties

PropertyValue

Antimony

10 - 14 %

Show Material materials with Antimony of 10 - 14 %

Lead

86 %

Show Material materials with Lead of 86 %