Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Melting point | 185 - 320 °C Show Material materials with Melting point of 185 - 320 °C | Typical for Lead Tin | |
Specific heat capacity | 23.0 °C | 213 - 239 J/(kg·K) Show Material materials with Specific heat capacity of 213 - 239 J/(kg·K) | Typical for Lead Tin |
Thermal conductivity | 23.0 °C | 35 - 57 W/(m·K) Show Material materials with Thermal conductivity of 35 - 57 W/(m·K) | Typical for Lead Tin |
Chemical properties
Property | Value |
---|---|
Antimony | 0.08 - 0.12 % Show Material materials with Antimony of 0.08 - 0.12 % |
Arsenic | 1E-3 % Show Material materials with Arsenic of 1E-3 % |
Bismuth | 0.03 % Show Material materials with Bismuth of 0.03 % |
Cadmium | 1E-3 % Show Material materials with Cadmium of 1E-3 % |
Copper | 3E-3 % Show Material materials with Copper of 3E-3 % |
Lead | 99.61 % Show Material materials with Lead of 99.61 % |
Nickel | 1E-3 % Show Material materials with Nickel of 1E-3 % |
Silver | 5E-3 % Show Material materials with Silver of 5E-3 % |
Tellurium | 2E-3 % Show Material materials with Tellurium of 2E-3 % |
Tin | 0.17 - 0.23 % Show Material materials with Tin of 0.17 - 0.23 % |
Zinc | 1E-3 % Show Material materials with Zinc of 1E-3 % |