General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 11.34 g/cm³ Show Material materials with Density of 11.34 g/cm³ | Typical for Pure/Low Alloyed Lead |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Poisson's ratio | 23.0 °C | 0.4 [-] Show Material materials with Poisson's ratio of 0.4 [-] | Typical for Pure/Low Alloyed Lead |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Melting point | 327 °C Show Material materials with Melting point of 327 °C | Typical for Pure/Low Alloyed Lead | |
Specific heat capacity | 23.0 °C | 112 - 134 J/(kg·K) Show Material materials with Specific heat capacity of 112 - 134 J/(kg·K) | Typical for Pure/Low Alloyed Lead |
Thermal conductivity | 23.0 °C | 34 - 35 W/(m·K) Show Material materials with Thermal conductivity of 34 - 35 W/(m·K) | Typical for Pure/Low Alloyed Lead |
Chemical properties
Property | Value |
---|---|
Antimony | 3E-3 % Show Material materials with Antimony of 3E-3 % |
Arsenic | 0.15 - 0.18 % Show Material materials with Arsenic of 0.15 - 0.18 % |
Bismuth | 0.08 - 0.12 % Show Material materials with Bismuth of 0.08 - 0.12 % |
Cadmium | 1E-3 % Show Material materials with Cadmium of 1E-3 % |
Copper | 3E-3 % Show Material materials with Copper of 3E-3 % |
Lead | 99.56 % Show Material materials with Lead of 99.56 % |
Nickel | 1E-3 % Show Material materials with Nickel of 1E-3 % |
Silver | 3E-3 % Show Material materials with Silver of 3E-3 % |
Tellurium | 2E-3 % Show Material materials with Tellurium of 2E-3 % |
Tin | 0.1 - 0.13 % Show Material materials with Tin of 0.1 - 0.13 % |
Zinc | 1E-3 % Show Material materials with Zinc of 1E-3 % |