EN 12844 Grade G-ZnAl6Cu1 cast condition

Want to keep this datasheet? Save it now in your required format

Description

The material G-ZnAl6Cu1, material NR. 2.2161, characteristic Z 610, one uses for castingtechnically difficult sand and ingot castings.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

6.5 g/cm³

Show Material materials with Density of 6.5 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

20.0 °C

130 GPa

Show Material materials with Elastic modulus of 130 GPa

Elongation

20.0 °C

1 - 3 %

Show Material materials with Elongation of 1 - 3 %

Hardness, Brinell

20.0 °C

80 - 90 [-]

Show Material materials with Hardness, Brinell of 80 - 90 [-]

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Zinc Aluminium

Tensile strength

20.0 °C

180 - 260 MPa

Show Material materials with Tensile strength of 180 - 260 MPa

Yield strength Rp0.2

20.0 °C

150 - 200 MPa

Show Material materials with Yield strength Rp0.2 of 150 - 200 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

2.2E-5 - 2.8E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2.2E-5 - 2.8E-5 1/K

Typical for Zinc Aluminium

Melting point

375 - 485 °C

Show Material materials with Melting point of 375 - 485 °C

Typical for Zinc Aluminium

Specific heat capacity

20.0 °C

452 J/(kg·K)

Show Material materials with Specific heat capacity of 452 J/(kg·K)

Thermal conductivity

20.0 °C

105 W/(m·K)

Show Material materials with Thermal conductivity of 105 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

20.0 °C

1.50E+7 - 1.60E+7 S/m

Show Material materials with Electrical conductivity of 1.50E+7 - 1.60E+7 S/m

Chemical properties

PropertyValue

Aluminium

5.6 - 6 %

Show Material materials with Aluminium of 5.6 - 6 %

Copper

1.2 - 1.6 %

Show Material materials with Copper of 1.2 - 1.6 %

Iron

0.08 %

Show Material materials with Iron of 0.08 %

Magnesium

5E-3 %

Show Material materials with Magnesium of 5E-3 %

Tin

2E-3 %

Show Material materials with Tin of 2E-3 %

Zinc

92.32 %

Show Material materials with Zinc of 92.32 %

Technological properties

Property
Processing methods

permanent mould casting, separately cast test sample