General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 10.1 g/cm³ Show Material materials with Density of 10.1 g/cm³ |
Mechanical
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Melting point | 235 - 305 °C Show Material materials with Melting point of 235 - 305 °C | Typical for Lead Antimony | |
Specific heat capacity | 23.0 °C | 130 - 159 J/(kg·K) Show Material materials with Specific heat capacity of 130 - 159 J/(kg·K) | Typical for Lead Antimony |
Thermal conductivity | 23.0 °C | 24 - 34 W/(m·K) Show Material materials with Thermal conductivity of 24 - 34 W/(m·K) | Typical for Lead Antimony |
Chemical properties
Property | Value |
---|---|
Antimony | 12 - 14 % Show Material materials with Antimony of 12 - 14 % |
Arsenic | 0.05 % Show Material materials with Arsenic of 0.05 % |
Cadmium | 0.05 % Show Material materials with Cadmium of 0.05 % |
Iron | 0.05 % Show Material materials with Iron of 0.05 % |
Lead | 86 - 88 % Show Material materials with Lead of 86 - 88 % |
Technological properties
Property | ||
---|---|---|
Processing methods | pressure die casting, separately cast test sample,pressure die casting |