General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 9.8 g/cm³ Show Material materials with Density of 9.8 g/cm³ |
Mechanical
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Melting point | 235 - 305 °C Show Material materials with Melting point of 235 - 305 °C | Typical for Lead Antimony | |
Specific heat capacity | 23.0 °C | 130 - 159 J/(kg·K) Show Material materials with Specific heat capacity of 130 - 159 J/(kg·K) | Typical for Lead Antimony |
Thermal conductivity | 23.0 °C | 24 - 34 W/(m·K) Show Material materials with Thermal conductivity of 24 - 34 W/(m·K) | Typical for Lead Antimony |
Chemical properties
Property | Value |
---|---|
Antimony | 9 - 11 % Show Material materials with Antimony of 9 - 11 % |
Arsenic | 0.05 % Show Material materials with Arsenic of 0.05 % |
Cadmium | 0.05 % Show Material materials with Cadmium of 0.05 % |
Iron | 0.05 % Show Material materials with Iron of 0.05 % |
Lead | 84 - 86 % Show Material materials with Lead of 84 - 86 % |
Tin | 4 - 6 % Show Material materials with Tin of 4 - 6 % |
Technological properties
Property | ||
---|---|---|
Processing methods | pressure die casting, separately cast test sample,pressure die casting |