Description

AgCu20 material is used as AC and DC switch for power and communications engineering with switching currents up to 10 A, isolated up to 25 A, more rarely at higher currents.

Related Standards

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

10.2 g/cm³

Show Material materials with Density of 10.2 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

20.0 °C

85 GPa

Show Material materials with Elastic modulus of 85 GPa

Hardness, Vickers

20.0 °C

130 [-]

Show Material materials with Hardness, Vickers of 130 [-]

Poisson's ratio

23.0 °C

0.37 [-]

Show Material materials with Poisson's ratio of 0.37 [-]

Typical for Silver

Shear modulus

23.0 °C

30 GPa

Show Material materials with Shear modulus of 30 GPa

Typical for Silver

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.9E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.9E-5 1/K

Typical for Silver

Melting point

962 °C

Show Material materials with Melting point of 962 °C

Typical for Silver

Specific heat capacity

23.0 °C

234 - 251 J/(kg·K)

Show Material materials with Specific heat capacity of 234 - 251 J/(kg·K)

Typical for Silver

Thermal conductivity

20.0 °C

335 W/(m·K)

Show Material materials with Thermal conductivity of 335 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

20.0 °C

4.60E+7 S/m

Show Material materials with Electrical conductivity of 4.60E+7 S/m

Electrical resistivity

20.0 °C

2.17E-8 Ω·m

Show Material materials with Electrical resistivity of 2.17E-8 Ω·m

Chemical properties

PropertyValue

Copper

20 %

Show Material materials with Copper of 20 %

Silver

80 %

Show Material materials with Silver of 80 %