General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 10.1 g/cm³ Show Material materials with Density of 10.1 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 20.0 °C | 140 GPa Show Material materials with Elastic modulus of 140 GPa | |
Elongation | 20.0 °C | 2 - 5 % Show Material materials with Elongation of 2 - 5 % | |
Poisson's ratio | 23.0 °C | 0.37 [-] Show Material materials with Poisson's ratio of 0.37 [-] | Typical for Silver |
Shear modulus | 23.0 °C | 30 GPa Show Material materials with Shear modulus of 30 GPa | Typical for Silver |
Tensile strength | 20.0 °C | 540 MPa Show Material materials with Tensile strength of 540 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.9E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.9E-5 1/K | Typical for Silver |
Melting point | 962 °C Show Material materials with Melting point of 962 °C | Typical for Silver | |
Specific heat capacity | 23.0 °C | 234 - 251 J/(kg·K) Show Material materials with Specific heat capacity of 234 - 251 J/(kg·K) | Typical for Silver |
Thermal conductivity | 20.0 °C | 150 W/(m·K) Show Material materials with Thermal conductivity of 150 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 20.0 °C | 1.90E+7 S/m Show Material materials with Electrical conductivity of 1.90E+7 S/m |
Electrical resistivity | 20.0 °C | 5.3E-8 Ω·m Show Material materials with Electrical resistivity of 5.3E-8 Ω·m |