AgZn5

Want to keep this datasheet? Save it now in your required format

Description

The addition of zinc (Zn) leads to a hardening of the silver-zinc alloy AgZn5, also Ag95Zn5 or 95Ag5Zn. With not too large proportions of the hardening metals, easily deformable alloys are obtained.

Related Standards

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

10.5 g/cm³

Show Material materials with Density of 10.5 g/cm³

Typical for Silver

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

83 GPa

Show Material materials with Elastic modulus of 83 GPa

Typical for Silver

Poisson's ratio

23.0 °C

0.37 [-]

Show Material materials with Poisson's ratio of 0.37 [-]

Typical for Silver

Shear modulus

23.0 °C

30 GPa

Show Material materials with Shear modulus of 30 GPa

Typical for Silver

Tensile strength

20.0 °C

190 MPa

Show Material materials with Tensile strength of 190 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.9E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.9E-5 1/K

Typical for Silver

Melting point

962 °C

Show Material materials with Melting point of 962 °C

Typical for Silver

Specific heat capacity

23.0 °C

234 - 251 J/(kg·K)

Show Material materials with Specific heat capacity of 234 - 251 J/(kg·K)

Typical for Silver

Thermal conductivity

23.0 °C

417 - 428 W/(m·K)

Show Material materials with Thermal conductivity of 417 - 428 W/(m·K)

Typical for Silver

Chemical properties

PropertyValue

Silver

95 %

Show Material materials with Silver of 95 %

Zinc

5 %

Show Material materials with Zinc of 5 %