Description

Gold (Au) is a reddish-yellow, in very thin films blue-green translucent, cubic crystallizing precious metal. It is one of the heaviest metals, is relatively soft and very elastic. Among all metals, it has the best hot and cold ductility and can be hammered down to foil up to 0.0001 mm thick. Gold, which does not oxidize even at higher temperatures, forms alloys with almost all metals. Even small alloy additions can significantly increase the strength and hardness of gold and change its color (white gold: Pt, Pd, Ni / color gold: Cu). The chemical properties of gold characterize the concept of the precious metal par excellence. Thus, at normal temperature, Au is not attacked by dry and moist air, water, oxygen, fluorine, iodine, sulfur, as well as the vast majority of acids, aqueous salt solutions and alkalis, regardless of the concentration. In the electrical industry (just under 10% of gold consumption), the material gold is used for switching contacts (dry circuits with the smallest currents and voltages), plug contacts, transistor and IC carriers, ultrafine wires for semiconductors and anodes. It is very ductile, corrosion-resistant, oxidation-resistant, has a tendency to cold sweat. Au is machineless and machinable, roll-galvanized galvanic and can be separated from the gas phase.

Related Standards

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

19.3 g/cm³

Show Material materials with Density of 19.3 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

20.0 °C

78 GPa

Show Material materials with Elastic modulus of 78 GPa

Elongation

20.0 °C

3 %

Show Material materials with Elongation of 3 %

Hardness, Vickers

20.0 °C

90 [-]

Show Material materials with Hardness, Vickers of 90 [-]

Poisson's ratio

20.0 °C

0.42 [-]

Show Material materials with Poisson's ratio of 0.42 [-]

Shear modulus

20.0 °C

28 GPa

Show Material materials with Shear modulus of 28 GPa

Tensile strength

20.0 °C

300 MPa

Show Material materials with Tensile strength of 300 MPa

Yield strength

20.0 °C

260 MPa

Show Material materials with Yield strength of 260 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

100.0 °C

1.39E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.39E-5 1/K

200.0 °C

1.48E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.48E-5 1/K

300.0 °C

1.52E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.52E-5 1/K

400.0 °C

1.53E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.53E-5 1/K

500.0 °C

1.55E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.55E-5 1/K

600.0 °C

1.57E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.57E-5 1/K

700.0 °C

1.59E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.59E-5 1/K

800.0 °C

1.62E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.62E-5 1/K

Melting point

1064 °C

Show Material materials with Melting point of 1064 °C

Typical for Gold

Specific heat capacity

23.0 °C

126 - 138 J/(kg·K)

Show Material materials with Specific heat capacity of 126 - 138 J/(kg·K)

Typical for Gold

Thermal conductivity

-233.0 °C

420 W/(m·K)

Show Material materials with Thermal conductivity of 420 W/(m·K)

-173.0 °C

360 W/(m·K)

Show Material materials with Thermal conductivity of 360 W/(m·K)

-73.0 °C

326 W/(m·K)

Show Material materials with Thermal conductivity of 326 W/(m·K)

20.0 °C

312 W/(m·K)

Show Material materials with Thermal conductivity of 312 W/(m·K)

127.0 °C

309 W/(m·K)

Show Material materials with Thermal conductivity of 309 W/(m·K)

327.0 °C

296 W/(m·K)

Show Material materials with Thermal conductivity of 296 W/(m·K)

527.0 °C

284 W/(m·K)

Show Material materials with Thermal conductivity of 284 W/(m·K)

727.0 °C

271 W/(m·K)

Show Material materials with Thermal conductivity of 271 W/(m·K)

Unlock all property charts

Electrical

PropertyTemperatureValue

Electrical conductivity

20.0 °C

4.30E+7 S/m

Show Material materials with Electrical conductivity of 4.30E+7 S/m

Electrical resistivity

20.0 °C

2.3E-8 - 2.9E-8 Ω·m

Show Material materials with Electrical resistivity of 2.3E-8 - 2.9E-8 Ω·m

Chemical properties

PropertyValue

Gold

99.99 %

Show Material materials with Gold of 99.99 %