AuAg14Pt6.9 precipitation hardened (+P)

Want to keep this datasheet? Save it now in your required format

Description

The gold-silver-platinum alloy AuAg14Pt6.9, also Au79,1Ag14Pt6.9 or 79.1Au14Ag6.9Pt, is mainly used in the dental field.

Related Standards

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

19.3 g/cm³

Show Material materials with Density of 19.3 g/cm³

Typical for Gold

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

74 - 81 GPa

Show Material materials with Elastic modulus of 74 - 81 GPa

Typical for Gold

Elongation

20.0 °C

40 %

Show Material materials with Elongation of 40 %

Hardness, Vickers

20.0 °C

60 [-]

Show Material materials with Hardness, Vickers of 60 [-]

Poisson's ratio

23.0 °C

0.42 [-]

Show Material materials with Poisson's ratio of 0.42 [-]

Typical for Gold

Shear modulus

23.0 °C

26 GPa

Show Material materials with Shear modulus of 26 GPa

Typical for Gold

Tensile strength

20.0 °C

230 MPa

Show Material materials with Tensile strength of 230 MPa

Yield strength Rp0.2

20.0 °C

80 MPa

Show Material materials with Yield strength Rp0.2 of 80 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.4E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.4E-5 1/K

Typical for Gold

Melting point

1064 °C

Show Material materials with Melting point of 1064 °C

Typical for Gold

Specific heat capacity

23.0 °C

126 - 138 J/(kg·K)

Show Material materials with Specific heat capacity of 126 - 138 J/(kg·K)

Typical for Gold

Thermal conductivity

23.0 °C

292 - 316 W/(m·K)

Show Material materials with Thermal conductivity of 292 - 316 W/(m·K)

Typical for Gold

Chemical properties

PropertyValue

Gold

79.1 %

Show Material materials with Gold of 79.1 %

Platinum

6.9 %

Show Material materials with Platinum of 6.9 %

Silver

14 %

Show Material materials with Silver of 14 %