General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 16.5 g/cm³ Show Material materials with Density of 16.5 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 20.0 °C | 87 GPa Show Material materials with Elastic modulus of 87 GPa | |
Hardness, Vickers | 20.0 °C | 40 [-] Show Material materials with Hardness, Vickers of 40 [-] | |
Poisson's ratio | 23.0 °C | 0.42 [-] Show Material materials with Poisson's ratio of 0.42 [-] | Typical for Gold |
Shear modulus | 20.0 °C | 31 GPa Show Material materials with Shear modulus of 31 GPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 300.0 °C | 1.62E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.62E-5 1/K | |
Melting point | 1064 °C Show Material materials with Melting point of 1064 °C | Typical for Gold | |
Specific heat capacity | 23.0 °C | 126 - 138 J/(kg·K) Show Material materials with Specific heat capacity of 126 - 138 J/(kg·K) | Typical for Gold |
Thermal conductivity | 20.0 °C | 75 W/(m·K) Show Material materials with Thermal conductivity of 75 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 20.0 °C | 1.00E+7 S/m Show Material materials with Electrical conductivity of 1.00E+7 S/m |
Electrical resistivity | 20.0 °C | 9.5E-8 - 1E-7 Ω·m Show Material materials with Electrical resistivity of 9.5E-8 - 1E-7 Ω·m |