General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 16 g/cm³ Show Material materials with Density of 16 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 20.0 °C | 93 GPa Show Material materials with Elastic modulus of 93 GPa | |
Hardness, Vickers | 20.0 °C | 110 [-] Show Material materials with Hardness, Vickers of 110 [-] | |
Poisson's ratio | 23.0 °C | 0.42 [-] Show Material materials with Poisson's ratio of 0.42 [-] | Typical for Gold |
Shear modulus | 20.0 °C | 35 GPa Show Material materials with Shear modulus of 35 GPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 300.0 °C | 1.54E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.54E-5 1/K | |
Melting point | 1064 °C Show Material materials with Melting point of 1064 °C | Typical for Gold | |
Specific heat capacity | 23.0 °C | 126 - 138 J/(kg·K) Show Material materials with Specific heat capacity of 126 - 138 J/(kg·K) | Typical for Gold |
Thermal conductivity | 20.0 °C | 46 W/(m·K) Show Material materials with Thermal conductivity of 46 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 20.0 °C | 6.20E+6 S/m Show Material materials with Electrical conductivity of 6.20E+6 S/m |
Electrical resistivity | 20.0 °C | 1.63E-7 - 1.64E-7 Ω·m Show Material materials with Electrical resistivity of 1.63E-7 - 1.64E-7 Ω·m |