AuAg5Pd15Pt7.5 precipitation hardened (+P)

.XLSX
.PDF
Save

Properties

Mechanical

Elongation A

18 % at 20 °C

Hardness, Vickers HV

125 [-] at 20 °C

Tensile strength Rm

410 MPa at 20 °C

Yield strength Rp0.2 Rp0.2

240 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Au

72.5 %

Pd

15 %

Pt

7.5 %

Ag

5 %

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Contact our suppliers

Select the region(s) and press “Contact suppliers“

China (5)
America (3)
Germany (6)
India (4)
Other regions