General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 15.6 g/cm³ Show Material materials with Density of 15.6 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 20.0 °C | 103 GPa Show Material materials with Elastic modulus of 103 GPa | |
Poisson's ratio | 23.0 °C | 0.42 [-] Show Material materials with Poisson's ratio of 0.42 [-] | Typical for Gold |
Shear modulus | 20.0 °C | 39 GPa Show Material materials with Shear modulus of 39 GPa | |
Tensile strength | 20.0 °C | 680 MPa Show Material materials with Tensile strength of 680 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 300.0 °C | 1.53E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.53E-5 1/K | |
Melting point | 1064 °C Show Material materials with Melting point of 1064 °C | Typical for Gold | |
Specific heat capacity | 23.0 °C | 126 - 138 J/(kg·K) Show Material materials with Specific heat capacity of 126 - 138 J/(kg·K) | Typical for Gold |
Thermal conductivity | 23.0 °C | 292 - 316 W/(m·K) Show Material materials with Thermal conductivity of 292 - 316 W/(m·K) | Typical for Gold |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical resistivity | 20.0 °C | 3.26E-7 - 3.42E-7 Ω·m Show Material materials with Electrical resistivity of 3.26E-7 - 3.42E-7 Ω·m |