General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 19.5 g/cm³ Show Material materials with Density of 19.5 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 20.0 °C | 95 GPa Show Material materials with Elastic modulus of 95 GPa | |
Hardness, Vickers | 20.0 °C | 80 [-] Show Material materials with Hardness, Vickers of 80 [-] | |
Poisson's ratio | 23.0 °C | 0.42 [-] Show Material materials with Poisson's ratio of 0.42 [-] | Typical for Gold |
Shear modulus | 23.0 °C | 26 GPa Show Material materials with Shear modulus of 26 GPa | Typical for Gold |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.4E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.4E-5 1/K | Typical for Gold |
Melting point | 1064 °C Show Material materials with Melting point of 1064 °C | Typical for Gold | |
Specific heat capacity | 23.0 °C | 126 - 138 J/(kg·K) Show Material materials with Specific heat capacity of 126 - 138 J/(kg·K) | Typical for Gold |
Thermal conductivity | 20.0 °C | 54 W/(m·K) Show Material materials with Thermal conductivity of 54 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 20.0 °C | 8.00E+6 S/m Show Material materials with Electrical conductivity of 8.00E+6 S/m |
Electrical resistivity | 20.0 °C | 1.25E-7 Ω·m Show Material materials with Electrical resistivity of 1.25E-7 Ω·m |