Mechanical
Property | Temperature | Value |
---|---|---|
Hardness, Vickers, 5 | 20.0 °C | 95 [-] Show Material materials with Hardness, Vickers, 5 of 95 [-] |
Thermal
Property | Value |
---|---|
Melting point | 1040 °C Show Material materials with Melting point of 1040 °C |
Chemical properties
Property | Value |
---|---|
Copper | 4.1 % Show Material materials with Copper of 4.1 % |
Gold | 75.7 % Show Material materials with Gold of 75.7 % |
Palladium | 3.3 % Show Material materials with Palladium of 3.3 % |
Platinum | 2 % Show Material materials with Platinum of 2 % |
Silver | 15 % Show Material materials with Silver of 15 % |
Zinc | 2 % Show Material materials with Zinc of 2 % |