General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 12 g/cm³ Show Material materials with Density of 12 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 20.0 °C | 121 GPa Show Material materials with Elastic modulus of 121 GPa | |
Elongation | 20.0 °C | 3 % Show Material materials with Elongation of 3 % | |
Hardness, Vickers | 20.0 °C | 210 [-] Show Material materials with Hardness, Vickers of 210 [-] | |
Poisson's ratio | 23.0 °C | 0.39 [-] Show Material materials with Poisson's ratio of 0.39 [-] | Typical for Palladium |
Shear modulus | 20.0 °C | 50 GPa Show Material materials with Shear modulus of 50 GPa | |
Tensile strength | 20.0 °C | 480 MPa Show Material materials with Tensile strength of 480 MPa | |
Yield strength | 20.0 °C | 400 MPa Show Material materials with Yield strength of 400 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 50.0 °C | 1.18E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.18E-5 1/K | |
100.0 °C | 1.19E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.19E-5 1/K | ||
200.0 °C | 1.21E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.21E-5 1/K | ||
300.0 °C | 1.23E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.23E-5 1/K | ||
400.0 °C | 1.26E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.26E-5 1/K | ||
500.0 °C | 1.28E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.28E-5 1/K | ||
600.0 °C | 1.3E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.3E-5 1/K | ||
700.0 °C | 1.32E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.32E-5 1/K | ||
800.0 °C | 1.34E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.34E-5 1/K | ||
900.0 °C | 1.36E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.36E-5 1/K | ||
1000.0 °C | 1.39E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.39E-5 1/K | ||
Melting point | 1553 °C Show Material materials with Melting point of 1553 °C | Typical for Palladium | |
Specific heat capacity | 23.0 °C | 236 - 248 J/(kg·K) Show Material materials with Specific heat capacity of 236 - 248 J/(kg·K) | Typical for Palladium |
Thermal conductivity | 20.0 °C | 75 W/(m·K) Show Material materials with Thermal conductivity of 75 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical resistivity | 20.0 °C | 1.01E-7 Ω·m Show Material materials with Electrical resistivity of 1.01E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Palladium | 99.9 % Show Material materials with Palladium of 99.9 % |