General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 12.16 g/cm³ Show Material materials with Density of 12.16 g/cm³ | Typical for Palladium |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 121 GPa Show Material materials with Elastic modulus of 121 GPa | Typical for Palladium |
Elongation | 20.0 °C | 29 % Show Material materials with Elongation of 29 % | |
Hardness, Vickers, 5 | 20.0 °C | 160 [-] Show Material materials with Hardness, Vickers, 5 of 160 [-] | |
Poisson's ratio | 23.0 °C | 0.39 [-] Show Material materials with Poisson's ratio of 0.39 [-] | Typical for Palladium |
Shear modulus | 23.0 °C | 42 GPa Show Material materials with Shear modulus of 42 GPa | Typical for Palladium |
Tensile strength | 20.0 °C | 630 MPa Show Material materials with Tensile strength of 630 MPa | |
Yield strength Rp0.2 | 20.0 °C | 340 MPa Show Material materials with Yield strength Rp0.2 of 340 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.1E-5 - 1.4E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.1E-5 - 1.4E-5 1/K | Typical for Palladium |
Melting point | 1553 °C Show Material materials with Melting point of 1553 °C | Typical for Palladium | |
Specific heat capacity | 23.0 °C | 236 - 248 J/(kg·K) Show Material materials with Specific heat capacity of 236 - 248 J/(kg·K) | Typical for Palladium |
Thermal conductivity | 23.0 °C | 60 - 76 W/(m·K) Show Material materials with Thermal conductivity of 60 - 76 W/(m·K) | Typical for Palladium |