General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 11.4 g/cm³ Show Material materials with Density of 11.4 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 20.0 °C | 135 GPa Show Material materials with Elastic modulus of 135 GPa | |
Elongation | 20.0 °C | 2 % Show Material materials with Elongation of 2 % | |
Hardness, Vickers | 20.0 °C | 205 [-] Show Material materials with Hardness, Vickers of 205 [-] | |
Poisson's ratio | 23.0 °C | 0.39 [-] Show Material materials with Poisson's ratio of 0.39 [-] | Typical for Palladium |
Shear modulus | 20.0 °C | 47 GPa Show Material materials with Shear modulus of 47 GPa | |
Tensile strength | 20.0 °C | 700 MPa Show Material materials with Tensile strength of 700 MPa | |
Yield strength Rp0.2 | 20.0 °C | 690 MPa Show Material materials with Yield strength Rp0.2 of 690 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 300.0 °C | 1.4E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.4E-5 1/K | |
Melting point | 1553 °C Show Material materials with Melting point of 1553 °C | Typical for Palladium | |
Specific heat capacity | 23.0 °C | 236 - 248 J/(kg·K) Show Material materials with Specific heat capacity of 236 - 248 J/(kg·K) | Typical for Palladium |
Thermal conductivity | 23.0 °C | 60 - 76 W/(m·K) Show Material materials with Thermal conductivity of 60 - 76 W/(m·K) | Typical for Palladium |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical resistivity | 20.0 °C | 4.13E-7 Ω·m Show Material materials with Electrical resistivity of 4.13E-7 Ω·m |