PdCd20

Want to keep this datasheet? Save it now in your required format

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValue

Tensile strength

20.0 °C

540 MPa

Show Material materials with Tensile strength of 540 MPa

Chemical properties

PropertyValue

Cadmium

20 %

Show Material materials with Cadmium of 20 %

Palladium

80 %

Show Material materials with Palladium of 80 %