General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 11.4 g/cm³ Show Material materials with Density of 11.4 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 20.0 °C | 172 GPa Show Material materials with Elastic modulus of 172 GPa | |
Hardness, Vickers | 20.0 °C | 100 [-] Show Material materials with Hardness, Vickers of 100 [-] | |
Poisson's ratio | 23.0 °C | 0.39 [-] Show Material materials with Poisson's ratio of 0.39 [-] | Typical for Palladium |
Shear modulus | 20.0 °C | 50 GPa Show Material materials with Shear modulus of 50 GPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 300.0 °C | 1.26E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.26E-5 1/K | |
Melting point | 1553 °C Show Material materials with Melting point of 1553 °C | Typical for Palladium | |
Specific heat capacity | 23.0 °C | 236 - 248 J/(kg·K) Show Material materials with Specific heat capacity of 236 - 248 J/(kg·K) | Typical for Palladium |
Thermal conductivity | 20.0 °C | 17 W/(m·K) Show Material materials with Thermal conductivity of 17 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 20.0 °C | 2.60E+6 S/m Show Material materials with Electrical conductivity of 2.60E+6 S/m |
Electrical resistivity | 20.0 °C | 4.03E-7 Ω·m Show Material materials with Electrical resistivity of 4.03E-7 Ω·m |