General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 10.5 g/cm³ Show Material materials with Density of 10.5 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 20.0 °C | 149 GPa Show Material materials with Elastic modulus of 149 GPa | |
Hardness, Vickers | 20.0 °C | 220 [-] Show Material materials with Hardness, Vickers of 220 [-] | |
Poisson's ratio | 23.0 °C | 0.39 [-] Show Material materials with Poisson's ratio of 0.39 [-] | Typical for Palladium |
Shear modulus | 23.0 °C | 42 GPa Show Material materials with Shear modulus of 42 GPa | Typical for Palladium |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 300.0 °C | 1.36E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.36E-5 1/K | |
Melting point | 1553 °C Show Material materials with Melting point of 1553 °C | Typical for Palladium | |
Specific heat capacity | 23.0 °C | 236 - 248 J/(kg·K) Show Material materials with Specific heat capacity of 236 - 248 J/(kg·K) | Typical for Palladium |
Thermal conductivity | 20.0 °C | 38 W/(m·K) Show Material materials with Thermal conductivity of 38 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 20.0 °C | 3.00E+6 S/m Show Material materials with Electrical conductivity of 3.00E+6 S/m |
Electrical resistivity | 20.0 °C | 3.33E-7 Ω·m Show Material materials with Electrical resistivity of 3.33E-7 Ω·m |