Description

The group of platinum metals includes the elements ruthenium (Ru), rhodium (Rh), palladium (Pd) (light platinum metals with densities around 12 g/cm³) as well as osmium (Os), iridium (Ir) and platinum (Pt) ( heavy platinum metals with densities up to 22 g/cm³). Platinum is a gray-white malleable metal that melts at 1772°C and has a boiling point of 3827°C. Platinum is machinable, roll-plating galvanic and can be separated from the gas phase. Application: Jewelery, in the automotive, chemical, petrochemical and pharmaceutical industries. Other important fields of application are the glass industry (melting furnaces, spinnerets, electrodes, crucibles for melt digestion of minerals and ferroalloys (also in fine grain stabilized form), crucibles and trays for the ashing and coking of organic matter (also in fine grain stabilized form), for peeling and evaporation of liquids, for electrodes in electroanalysis and potential measurement as well as for porous discs in filtration. Pt is also used as contact material. Pt has almost exactly the same coefficient of expansion as glass, so that it can melt completely tightly into glass and the electrical measuring technique (Pt and Pt / Rh thermocouples). Laboratory equipment such as pots and bowls are hardly made of pure platinum anymore.

Related Standards

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

21.5 g/cm³

Show Material materials with Density of 21.5 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

20.0 °C

170 GPa

Show Material materials with Elastic modulus of 170 GPa

Elongation

20.0 °C

3 %

Show Material materials with Elongation of 3 %

Hardness, Vickers

20.0 °C

98 [-]

Show Material materials with Hardness, Vickers of 98 [-]

Poisson's ratio

20.0 °C

0.39 [-]

Show Material materials with Poisson's ratio of 0.39 [-]

Shear modulus

20.0 °C

66 GPa

Show Material materials with Shear modulus of 66 GPa

Tensile strength

20.0 °C

300 MPa

Show Material materials with Tensile strength of 300 MPa

Yield strength

20.0 °C

290 MPa

Show Material materials with Yield strength of 290 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

100.0 °C

9.1E-6 1/K

Show Material materials with Coefficient of thermal expansion of 9.1E-6 1/K

200.0 °C

9.2E-6 1/K

Show Material materials with Coefficient of thermal expansion of 9.2E-6 1/K

300.0 °C

9.3E-6 1/K

Show Material materials with Coefficient of thermal expansion of 9.3E-6 1/K

400.0 °C

9.5E-6 1/K

Show Material materials with Coefficient of thermal expansion of 9.5E-6 1/K

500.0 °C

9.6E-6 1/K

Show Material materials with Coefficient of thermal expansion of 9.6E-6 1/K

600.0 °C

9.7E-6 1/K

Show Material materials with Coefficient of thermal expansion of 9.7E-6 1/K

700.0 °C

9.9E-6 1/K

Show Material materials with Coefficient of thermal expansion of 9.9E-6 1/K

800.0 °C

1E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1E-5 1/K

900.0 °C

1.01E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.01E-5 1/K

1000.0 °C

1.03E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.03E-5 1/K

1100.0 °C

1.05E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.05E-5 1/K

1200.0 °C

1.06E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.06E-5 1/K

1300.0 °C

1.08E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.08E-5 1/K

1400.0 °C

1.1E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.1E-5 1/K

1500.0 °C

1.12E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.12E-5 1/K

1600.0 °C

1.14E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.14E-5 1/K

Melting point

1769 °C

Show Material materials with Melting point of 1769 °C

Typical for Platinum

Specific heat capacity

23.0 °C

136 J/(kg·K)

Show Material materials with Specific heat capacity of 136 J/(kg·K)

Typical for Platinum

Thermal conductivity

20.0 °C

74 W/(m·K)

Show Material materials with Thermal conductivity of 74 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

20.0 °C

9.40E+6 S/m

Show Material materials with Electrical conductivity of 9.40E+6 S/m

Electrical resistivity

20.0 °C

1.09E-7 Ω·m

Show Material materials with Electrical resistivity of 1.09E-7 Ω·m

Chemical properties

PropertyValue

Platinum

99.5 - 99.99 %

Show Material materials with Platinum of 99.5 - 99.99 %