Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 20.0 °C | 4.50E+6 S/m Show Material materials with Electrical conductivity of 4.50E+6 S/m |
Electrical resistivity | 20.0 °C | 2.22E-7 Ω·m Show Material materials with Electrical resistivity of 2.22E-7 Ω·m |
General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 21.6 g/cm³ Show Material materials with Density of 21.6 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 20.0 °C | 220 GPa Show Material materials with Elastic modulus of 220 GPa |
Elongation | 20.0 °C | 25 - 37 % Show Material materials with Elongation of 25 - 37 % |
Hardness, Vickers | 20.0 °C | 110 [-] Show Material materials with Hardness, Vickers of 110 [-] |
Reduction of area | 20.0 °C | 28 - 97 % Show Material materials with Reduction of area of 28 - 97 % |
Tensile strength | 20.0 °C | 37 - 350 MPa Show Material materials with Tensile strength of 37 - 350 MPa |
Yield strength | 20.0 °C | 135 - 205 MPa Show Material materials with Yield strength of 135 - 205 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Melting point | 1785 °C Show Material materials with Melting point of 1785 °C | |
Thermal conductivity | 20.0 °C | 29 W/(m·K) Show Material materials with Thermal conductivity of 29 W/(m·K) |