General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 21.5 g/cm³ Show Material materials with Density of 21.5 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 20.0 °C | 190 GPa Show Material materials with Elastic modulus of 190 GPa | |
Hardness, Vickers | 20.0 °C | 150 [-] Show Material materials with Hardness, Vickers of 150 [-] | |
Poisson's ratio | 23.0 °C | 0.39 [-] Show Material materials with Poisson's ratio of 0.39 [-] | Typical for Platinum |
Shear modulus | 23.0 °C | 62 GPa Show Material materials with Shear modulus of 62 GPa | Typical for Platinum |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 8.8E-6 - 9.1E-6 1/K Show Material materials with Coefficient of thermal expansion of 8.8E-6 - 9.1E-6 1/K | Typical for Platinum |
Melting point | 1769 °C Show Material materials with Melting point of 1769 °C | Typical for Platinum | |
Specific heat capacity | 23.0 °C | 136 J/(kg·K) Show Material materials with Specific heat capacity of 136 J/(kg·K) | Typical for Platinum |
Thermal conductivity | 20.0 °C | 42 W/(m·K) Show Material materials with Thermal conductivity of 42 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 20.0 °C | 5.60E+6 S/m Show Material materials with Electrical conductivity of 5.60E+6 S/m |
Electrical resistivity | 20.0 °C | 1.79E-7 Ω·m Show Material materials with Electrical resistivity of 1.79E-7 Ω·m |