General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 20.3 g/cm³ Show Material materials with Density of 20.3 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 154 - 172 GPa Show Material materials with Elastic modulus of 154 - 172 GPa | Typical for Platinum |
Hardness, Vickers, 10 | 20.0 °C | 125 [-] Show Material materials with Hardness, Vickers, 10 of 125 [-] | |
Poisson's ratio | 23.0 °C | 0.39 [-] Show Material materials with Poisson's ratio of 0.39 [-] | Typical for Platinum |
Shear modulus | 23.0 °C | 62 GPa Show Material materials with Shear modulus of 62 GPa | Typical for Platinum |
Tensile strength | 20.0 °C | 360 MPa Show Material materials with Tensile strength of 360 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 8.8E-6 - 9.1E-6 1/K Show Material materials with Coefficient of thermal expansion of 8.8E-6 - 9.1E-6 1/K | Typical for Platinum |
Melting point | 1769 °C Show Material materials with Melting point of 1769 °C | Typical for Platinum | |
Specific heat capacity | 23.0 °C | 136 J/(kg·K) Show Material materials with Specific heat capacity of 136 J/(kg·K) | Typical for Platinum |
Thermal conductivity | 23.0 °C | 69 - 73 W/(m·K) Show Material materials with Thermal conductivity of 69 - 73 W/(m·K) | Typical for Platinum |