General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 21.4 g/cm³ Show Material materials with Density of 21.4 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 20.0 °C | 181 GPa Show Material materials with Elastic modulus of 181 GPa | |
Hardness, Vickers | 20.0 °C | 300 [-] Show Material materials with Hardness, Vickers of 300 [-] | |
Poisson's ratio | 23.0 °C | 0.39 [-] Show Material materials with Poisson's ratio of 0.39 [-] | Typical for Platinum |
Shear modulus | 23.0 °C | 62 GPa Show Material materials with Shear modulus of 62 GPa | Typical for Platinum |
Tensile strength | 20.0 °C | 950 MPa Show Material materials with Tensile strength of 950 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 300.0 °C | 8.9E-6 1/K Show Material materials with Coefficient of thermal expansion of 8.9E-6 1/K | |
Melting point | 1769 °C Show Material materials with Melting point of 1769 °C | Typical for Platinum | |
Specific heat capacity | 23.0 °C | 136 J/(kg·K) Show Material materials with Specific heat capacity of 136 J/(kg·K) | Typical for Platinum |
Thermal conductivity | 23.0 °C | 69 - 73 W/(m·K) Show Material materials with Thermal conductivity of 69 - 73 W/(m·K) | Typical for Platinum |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 20.0 °C | 2.30E+6 S/m Show Material materials with Electrical conductivity of 2.30E+6 S/m |
Electrical resistivity | 20.0 °C | 4.34E-7 Ω·m Show Material materials with Electrical resistivity of 4.34E-7 Ω·m |