General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 12.4 g/cm³ Show Material materials with Density of 12.4 g/cm³ | Typical for Rhodium |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 275 - 290 GPa Show Material materials with Elastic modulus of 275 - 290 GPa | Typical for Rhodium |
Hardness, Vickers | 20.0 °C | 178 [-] Show Material materials with Hardness, Vickers of 178 [-] | |
Poisson's ratio | 23.0 °C | 0.26 [-] Show Material materials with Poisson's ratio of 0.26 [-] | Typical for Rhodium |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 8.3E-6 - 8.5E-6 1/K Show Material materials with Coefficient of thermal expansion of 8.3E-6 - 8.5E-6 1/K | Typical for Rhodium |
Melting point | 1963 °C Show Material materials with Melting point of 1963 °C | Typical for Rhodium | |
Specific heat capacity | 23.0 °C | 254 J/(kg·K) Show Material materials with Specific heat capacity of 254 J/(kg·K) | Typical for Rhodium |
Thermal conductivity | 23.0 °C | 88 - 151 W/(m·K) Show Material materials with Thermal conductivity of 88 - 151 W/(m·K) | Typical for Rhodium |