Pd57.8Ag30.0Sn6.0In4.0ZnRu precipitation hardened (+P),soft annealed (+A)

.XLSX
.PDF
Save

Description

Palladium-based dental alloy of type Pd57.8AG30.0Sn6.0In4.0ZnRu for metal ceramics as well as for crowns and bridges.

Related Standards

Properties

Mechanical

Hardness, Vickers HV

160 - 300 [-] at 20 °C

Yield strength Rp0.2 Rp0.2

340 - 650 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

1.52E-5 1/K at 600 °C

Chemical properties

Element

Weight %

Comment

Pd

57.8 %

Ag

30 %

Sn

6 %

In

4 %

Zn

2 %