General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.19 g/cm³ Show Material materials with Density of 7.19 g/cm³ | Typical for Chromium |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 279 GPa Show Material materials with Elastic modulus of 279 GPa | Typical for Chromium |
Poisson's ratio | 23.0 °C | 0.21 [-] Show Material materials with Poisson's ratio of 0.21 [-] | Typical for Chromium |
Shear modulus | 23.0 °C | 115 GPa Show Material materials with Shear modulus of 115 GPa | Typical for Chromium |
Tensile strength | 20.0 °C | 760 MPa Show Material materials with Tensile strength of 760 MPa | |
Yield strength | 20.0 °C | 590 MPa Show Material materials with Yield strength of 590 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 4.9E-6 - 8.2E-6 1/K Show Material materials with Coefficient of thermal expansion of 4.9E-6 - 8.2E-6 1/K | Typical for Chromium |
Melting point | 1875 °C Show Material materials with Melting point of 1875 °C | Typical for Chromium | |
Specific heat capacity | 23.0 °C | 442 - 487 J/(kg·K) Show Material materials with Specific heat capacity of 442 - 487 J/(kg·K) | Typical for Chromium |
Thermal conductivity | 23.0 °C | 87 - 91 W/(m·K) Show Material materials with Thermal conductivity of 87 - 91 W/(m·K) | Typical for Chromium |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.25 % Show Material materials with Aluminium of 0.25 % |
Carbon | 0.1 % Show Material materials with Carbon of 0.1 % |
Chromium | 58 - 62 % Show Material materials with Chromium of 58 - 62 % |
Iron | 1 % Show Material materials with Iron of 1 % |
Manganese | 0.3 % Show Material materials with Manganese of 0.3 % |
Nitrogen | 0.3 % Show Material materials with Nitrogen of 0.3 % |
Phosphorus | 0.02 % Show Material materials with Phosphorus of 0.02 % |
Silicon | 1 % Show Material materials with Silicon of 1 % |
Sulfur | 0.02 % Show Material materials with Sulfur of 0.02 % |
Titanium | 0.5 % Show Material materials with Titanium of 0.5 % |