General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 9.6 g/cm³ Show Material materials with Density of 9.6 g/cm³ | Typical for Lead Antimony |
Mechanical
Property | Temperature | Value |
---|---|---|
Hardness, Brinell | 20.0 °C | 21 [-] Show Material materials with Hardness, Brinell of 21 [-] |
50.0 °C | 16 [-] Show Material materials with Hardness, Brinell of 16 [-] | |
120.0 °C | 14 [-] Show Material materials with Hardness, Brinell of 14 [-] | |
150.0 °C | 10 [-] Show Material materials with Hardness, Brinell of 10 [-] | |
Yield strength Rp0.2 | 20.0 °C | 43 MPa Show Material materials with Yield strength Rp0.2 of 43 MPa |
50.0 °C | 32 MPa Show Material materials with Yield strength Rp0.2 of 32 MPa | |
100.0 °C | 30 MPa Show Material materials with Yield strength Rp0.2 of 30 MPa | |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Melting point | 235 - 305 °C Show Material materials with Melting point of 235 - 305 °C | Typical for Lead Antimony | |
Specific heat capacity | 23.0 °C | 130 - 159 J/(kg·K) Show Material materials with Specific heat capacity of 130 - 159 J/(kg·K) | Typical for Lead Antimony |
Thermal conductivity | 23.0 °C | 24 - 34 W/(m·K) Show Material materials with Thermal conductivity of 24 - 34 W/(m·K) | Typical for Lead Antimony |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.01 % Show Material materials with Aluminium of 0.01 % |
Antimony | 14 - 16 % Show Material materials with Antimony of 14 - 16 % |
Arsenic | 0.6 % Show Material materials with Arsenic of 0.6 % |
Bismuth | 0.1 % Show Material materials with Bismuth of 0.1 % |
Copper | 0.7 % Show Material materials with Copper of 0.7 % |
Iron | 0.1 % Show Material materials with Iron of 0.1 % |
Tin | 9 - 11 % Show Material materials with Tin of 9 - 11 % |
Zinc | 0.01 % Show Material materials with Zinc of 0.01 % |