General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 10.3 g/cm³ Show Material materials with Density of 10.3 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Yield strength Rp0.2 | 20.0 °C | 27 - 39 MPa Show Material materials with Yield strength Rp0.2 of 27 - 39 MPa |
Thermal
Property | Value |
---|---|
Melting point | 260 °C Show Material materials with Melting point of 260 °C |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.01 % Show Material materials with Aluminium of 0.01 % |
Antimony | 9 - 11 % Show Material materials with Antimony of 9 - 11 % |
Arsenic | 0.25 % Show Material materials with Arsenic of 0.25 % |
Bismuth | 0.1 % Show Material materials with Bismuth of 0.1 % |
Copper | 0.7 % Show Material materials with Copper of 0.7 % |
Iron | 0.1 % Show Material materials with Iron of 0.1 % |
Tin | 5 - 7 % Show Material materials with Tin of 5 - 7 % |
Zinc | 0.01 % Show Material materials with Zinc of 0.01 % |