Mechanical
Property | Temperature | Value |
---|---|---|
Hardness, Brinell | 20.0 °C | 25 [-] Show Material materials with Hardness, Brinell of 25 [-] |
50.0 °C | 20 [-] Show Material materials with Hardness, Brinell of 20 [-] | |
120.0 °C | 12 [-] Show Material materials with Hardness, Brinell of 12 [-] | |
150.0 °C | 8 [-] Show Material materials with Hardness, Brinell of 8 [-] | |
Yield strength Rp0.2 | 20.0 °C | 61 MPa Show Material materials with Yield strength Rp0.2 of 61 MPa |
50.0 °C | 60 MPa Show Material materials with Yield strength Rp0.2 of 60 MPa | |
100.0 °C | 36 MPa Show Material materials with Yield strength Rp0.2 of 36 MPa | |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Melting point | 215 - 350 °C Show Material materials with Melting point of 215 - 350 °C | Typical for Tin Antimony | |
Thermal conductivity | 23.0 °C | 40 W/(m·K) Show Material materials with Thermal conductivity of 40 W/(m·K) | Typical for Tin Antimony |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.01 % Show Material materials with Aluminium of 0.01 % |
Antimony | 11 - 13 % Show Material materials with Antimony of 11 - 13 % |
Arsenic | 0.1 % Show Material materials with Arsenic of 0.1 % |
Bismuth | 0.08 % Show Material materials with Bismuth of 0.08 % |
Copper | 5 - 7 % Show Material materials with Copper of 5 - 7 % |
Iron | 0.1 % Show Material materials with Iron of 0.1 % |
Lead | 1 - 3 % Show Material materials with Lead of 1 - 3 % |
Zinc | 0.01 % Show Material materials with Zinc of 0.01 % |