Mechanical
Property | Temperature | Value |
---|---|---|
Hardness, Brinell | 20.0 °C | 22 [-] Show Material materials with Hardness, Brinell of 22 [-] |
50.0 °C | 17 [-] Show Material materials with Hardness, Brinell of 17 [-] | |
100.0 °C | 10 [-] Show Material materials with Hardness, Brinell of 10 [-] | |
120.0 °C | 11 [-] Show Material materials with Hardness, Brinell of 11 [-] | |
150.0 °C | 8 [-] Show Material materials with Hardness, Brinell of 8 [-] | |
Tensile strength | 20.0 °C | 77 MPa Show Material materials with Tensile strength of 77 MPa |
Yield strength Rp0.2 | 20.0 °C | 46 - 47 MPa Show Material materials with Yield strength Rp0.2 of 46 - 47 MPa |
50.0 °C | 44 MPa Show Material materials with Yield strength Rp0.2 of 44 MPa | |
100.0 °C | 27 MPa Show Material materials with Yield strength Rp0.2 of 27 MPa | |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Melting point | 215 - 350 °C Show Material materials with Melting point of 215 - 350 °C | Typical for Tin Antimony | |
Thermal conductivity | 23.0 °C | 40 W/(m·K) Show Material materials with Thermal conductivity of 40 W/(m·K) | Typical for Tin Antimony |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.01 % Show Material materials with Aluminium of 0.01 % |
Antimony | 7 - 8 % Show Material materials with Antimony of 7 - 8 % |
Arsenic | 0.1 % Show Material materials with Arsenic of 0.1 % |
Bismuth | 0.08 % Show Material materials with Bismuth of 0.08 % |
Cadmium | 0.05 % Show Material materials with Cadmium of 0.05 % |
Copper | 3 - 4 % Show Material materials with Copper of 3 - 4 % |
Iron | 0.1 % Show Material materials with Iron of 0.1 % |
Lead | 0.35 % Show Material materials with Lead of 0.35 % |
Zinc | 0.01 % Show Material materials with Zinc of 0.01 % |