General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 5 g/cm³ Show Material materials with Density of 5 g/cm³ | Typical for Zinc Aluminium |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Zinc Aluminium |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 2.2E-5 - 2.8E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.2E-5 - 2.8E-5 1/K | Typical for Zinc Aluminium |
Melting point | 375 - 485 °C Show Material materials with Melting point of 375 - 485 °C | Typical for Zinc Aluminium | |
Specific heat capacity | 23.0 °C | 393 - 525 J/(kg·K) Show Material materials with Specific heat capacity of 393 - 525 J/(kg·K) | Typical for Zinc Aluminium |
Thermal conductivity | 23.0 °C | 105 - 125 W/(m·K) Show Material materials with Thermal conductivity of 105 - 125 W/(m·K) | Typical for Zinc Aluminium |
Chemical properties
Property | Value |
---|---|
Aluminium | 5.6 - 6 % Show Material materials with Aluminium of 5.6 - 6 % |
Cadmium | 3E-3 % Show Material materials with Cadmium of 3E-3 % |
Copper | 1.2 - 1.6 % Show Material materials with Copper of 1.2 - 1.6 % |
Iron | 0.02 % Show Material materials with Iron of 0.02 % |
Lead | 3E-3 % Show Material materials with Lead of 3E-3 % |
Magnesium | 0.01 - 0.04 % Show Material materials with Magnesium of 0.01 - 0.04 % |
Silicon | 0.02 % Show Material materials with Silicon of 0.02 % |
Tin | 1E-3 % Show Material materials with Tin of 1E-3 % |