General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.13 g/cm³ Show Material materials with Density of 7.13 g/cm³ | Typical for Zinc |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 105 GPa Show Material materials with Elastic modulus of 105 GPa | Typical for Zinc |
Poisson's ratio | 23.0 °C | 0.25 [-] Show Material materials with Poisson's ratio of 0.25 [-] | Typical for Zinc |
Shear modulus | 23.0 °C | 42 GPa Show Material materials with Shear modulus of 42 GPa | Typical for Zinc |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 2.2E-5 - 2.8E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.2E-5 - 2.8E-5 1/K | Typical for Zinc |
Melting point | 380 - 420 °C Show Material materials with Melting point of 380 - 420 °C | Typical for Zinc | |
Specific heat capacity | 23.0 °C | 272 - 525 J/(kg·K) Show Material materials with Specific heat capacity of 272 - 525 J/(kg·K) | Typical for Zinc |
Thermal conductivity | 23.0 °C | 105 - 125 W/(m·K) Show Material materials with Thermal conductivity of 105 - 125 W/(m·K) | Typical for Zinc |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.01 - 0.04 % Show Material materials with Aluminium of 0.01 - 0.04 % |
Cadmium | 4E-3 % Show Material materials with Cadmium of 4E-3 % |
Chromium | 0.1 - 0.2 % Show Material materials with Chromium of 0.1 - 0.2 % |
Copper | 1 - 1.5 % Show Material materials with Copper of 1 - 1.5 % |
Iron | 0.04 % Show Material materials with Iron of 0.04 % |
Lead | 5E-3 % Show Material materials with Lead of 5E-3 % |
Magnesium | 0.02 % Show Material materials with Magnesium of 0.02 % |
Silicon | 0.04 % Show Material materials with Silicon of 0.04 % |
Tin | 3E-3 % Show Material materials with Tin of 3E-3 % |
Titanium | 0.15 - 0.25 % Show Material materials with Titanium of 0.15 - 0.25 % |