General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 9.8 g/cm³ Show Material materials with Density of 9.8 g/cm³ |
Mechanical
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Melting point | 235 - 305 °C Show Material materials with Melting point of 235 - 305 °C | Typical for Lead Antimony | |
Specific heat capacity | 23.0 °C | 130 - 159 J/(kg·K) Show Material materials with Specific heat capacity of 130 - 159 J/(kg·K) | Typical for Lead Antimony |
Thermal conductivity | 23.0 °C | 24 - 34 W/(m·K) Show Material materials with Thermal conductivity of 24 - 34 W/(m·K) | Typical for Lead Antimony |
Chemical properties
Technological properties
Property | ||
---|---|---|
Processing methods | pressure die casting, separately cast test sample |