General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 8.94 g/cm³ Show Material materials with Density of 8.94 g/cm³ |
Mechanical
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.69E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.69E-5 1/K |
Specific heat capacity | 23.0 °C | 385 J/(kg·K) Show Material materials with Specific heat capacity of 385 J/(kg·K) |
Thermal conductivity | 23.0 °C | 385 W/(m·K) Show Material materials with Thermal conductivity of 385 W/(m·K) |