the first trading company for aluminum semi-finished products in Switzerland. Today Allega is the leading, specialized service center for aluminum applications in the fields of industry, metal construction, facades, aviation and commercial vehicles.
Headquarters
Niederglatt, Switzerland
Website
Type
Distributor
Certifications
ISO 9001
, EN 9120
, ISO 14001
, ISO 45001
Grade | Shape | ||
---|---|---|---|
AA 7122 | Rod, Tube, Profile | AA 7122, EN AW-7122, DIN AlZnMgCu | EN 573-3 |
AA 7175 | Sheet, Profile | AA 7175, EN AW-7175 | |
EN AW-1050A | Sheet, Profile | EN AW-1050A, DIN Al99.5 | EN 573-1, EN 573-3 |
EN AW-2024 | Sheet, Profile | EN AW-2024 | |
EN AW-2124 | Sheet, Profile | EN AW-2124 | |
EN AW-2214 | Sheet, Profile | EN AW-2214 | |
EN AW-2618 | Sheet, Profile | EN AW-2618 | |
EN AW-3105 | Sheet, Profile | EN AW-3105, DIN AlMn0.5Mg0.5 | EN 1396, EN 573-1, EN 573-3 |
EN AW-5005 | Sheet, Profile | EN AW-5005, DIN AlMg1 | EN 602, EN 485-4, EN 573-3, EN 485-2, EN 1396, EN 573-1 |
EN AW-5083 | Sheet, Plate, Profile | EN AW-5083, DIN AlMg4.5Mn0.7 | EN 602, EN 485-4, EN 485-3, EN 573-3, EN 485-2, EN 573-1 |