We manufacture stainless steels and nickel alloys with diameters starting less than one tenth of a millimeter up to over one meter. Tradition, innovation and state-of-the-art plant engineering have been the basis of our products
Headquarters
Freital, Germany
Website
Type
Manufacturer and Processor
Certifications
ISO 9001
, ISO 14001
, ISO 50001
, AD 2000
, KTA 1401
, KTA 3201.1
, KTA 3211.1
, IATF 16949
Grade | Shape | ||
---|---|---|---|
EN 1.4005 | Wire, Bar, Forging | EN 1.4005, AISI 416, UNS S41600 | |
EN 1.4006 | Wire, Bar, Forging | EN 1.4006, AISI 410, UNS S41000 | |
EN 1.4021 | Wire, Bar, Forging | EN 1.4021, AISI 420, UNS S42000 | |
EN 1.4057 | Wire, Bar, Forging | EN 1.4057, AISI 431, UNS S43100 | |
EN 1.4109 | Wire, Bar, Forging | EN 1.4109, AISI 440A, UNS S44002 | |
EN 1.4112 | Wire, Bar, Forging | EN 1.4112, AISI 440B, UNS S44003 | |
EN 1.4125 | Wire, Bar, Forging | EN 1.4125, AISI 440C, UNS S44004 | |
EN 1.4313 | Wire, Bar, Forging | EN 1.4313, AISI 415, UNS S41500 | |
EN 1.4404 | Wire, Bar, Forging | EN 1.4404, AISI 316L, UNS S31603 | |
EN 1.4406 | Wire, Bar, Forging | EN 1.4406, AISI 316LN, UNS S31653 | |