EZM Edelstahlzieherei Mark GmbH

Claim this profile

About EZM Edelstahlzieherei Mark GmbH

EZM Edelstahlzieherei Mark GmbH is a manufacturer and international operating supplier of bright steel and profiles made of steel and titanium, focusing on applications in automotive engineering, machine construction, energy engineering and medical equipment.

Company profile

Headquarters

Wetter,North Rhine-Westphalia, Germany

Type

Manufacturer, Processor and Distributor

Certifications

IATF 16949

, ISO 9001

, ISO 14001

Grades provided by the supplier

Grade Shape Equivalent Materials Standard / Norm 

EN 1.3965

Bar, Profile

EN 1.3965

EN 1.4021

Wire, Bar, Sheet

EN 1.4021, AISI 420A, UNS S42000

ASTM A193, ASTM A194, ASTM A276, ASTM A479, ASTM F899, AMS 5848, ASTM A240, ASTM A182, A5.9 ER218

EN 1.4034

Wire, Bar, Sheet

EN 1.4034, AISI 420C, UNS S42000

ISO 7153-1, ASTM F899

EN 1.4108

Wire, Bar, Sheet

EN 1.4108, UNS S42027

ASTM F899

EN 1.4112

Wire, Bar, Sheet

EN 1.4112, AISI 440B, UNS S44003

EN 1.4197

Wire, Bar, Sheet

EN 1.4197, AISI 420F

ASTM F899

EN 1.4301

Wire, Bar, Sheet

EN 1.4301, AISI 304, UNS S30400

ISO 7153-1, ASTM F899

EN 1.4305

Wire, Bar, Sheet

EN 1.4305, AISI 303, UNS S30300

ISO 7153-1, ASTM F899

EN 1.4306

Wire, Bar, Sheet

EN 1.4306, AISI 304L, UNS S30403

ISO 7153-1

EN 1.4310

Wire, Bar, Sheet

EN 1.4310, AISI 302, AISI 301, UNS S30200

ISO 7153-1, ASTM F899

Showing 1 to 10 of 161 entries

Previous

1
2
3
...
17

Next

Locations

Germany

Germany

Auf der Bleiche 26

58300 Wetter,North Rhine-Westphalia

(+49)23359770

Hungary

Hungary

Mr. Zoltán Czégény,1.Szava

2621 Veröce

(+36)207733104

India

India

706, Shakuntala Apartment,59 Nehru Place

110019 New Delhi

(+91)1146074908

Switzerland

Switzerland

Industriestrasse 20/Bronschhofen

9501 Wil

(+41)719136510

Turkey

Turkey

Adalet mah. Anadolu caddesi,Megapol Tower No. 41/81

35530 İzmir

(+90)5355576818

United States

United States

2518 W. Maypole

60612 Chicago,Illinois

(+1)7735398501