Powerhouse, backbone, driver of innovation: GMH Gruppe's steel moves whole industries throughout the world. Learn here about the role it plays in current and future technological challenges.
Headquarters
Georgsmarienhütte,Lower Saxony, Germany
Type
Manufacturer and Processor
Certifications
ISO 9001
Grade | Shape | ||
---|---|---|---|
DIN 1.0038 | Bar | DIN 1.0038, EN S255JR | DIN EN 10060 |
DIN 1.0401 | Bar | DIN 1.0401, EN C15 | DIN EN 10060 |
DIN 1.0468 | Bar | DIN 1.0468, EN C10 | DIN EN 10060 |
DIN 1.0570 | Bar | DIN 1.0570, EN S355J2 | DIN EN 10060 |
DIN 1.1133 | Bar | DIN 1.1133, EN 20Mn5 | DIN EN 10060 |
DIN 1.1191 | Bar | DIN 1.1191, EN C45E | DIN EN 10060 |
DIN 1.1206 | Rod | DIN 1.1206, EN C50E | DIN EN 10277 |
DIN 1.5094 | Rod | DIN 1.5094, EN 38MnS6 | DIN EN 10277 |
DIN 1.5511 | Bar | DIN 1.5511, EN 35B2 | DIN EN 10060 |
DIN 1.5531 | Bar | DIN 1.5531, EN 30MnB5 | DIN EN 10060 |