Metal Alloys Corporation - one of the leading manufacturer of Copper and Copper Alloys Cast, Extruded and Drawn products, viz. Billets/Ingots, Mother Shells, Tubes/Pipes, Hollow/Solid Rods, Sections, Profiles etc.
Headquarters
Jamnagar, India
Type
Manufacturer, Processor and Distributor
Certifications
ISO 9001
Grade | Shape | ||
---|---|---|---|
BS CZ124 | Rod | BS CZ124, JIS C3713 | JIS H3100 |
EN CuZn36Pb3 | Rod | EN CuZn36Pb3, UNS C36000, EN CW603N, BS CZ124, DIN 2.0375 | |
EN CW510L | Tube | EN CW510L, EN CuZn42 | |
UNS C26000 | Tube, Pipe | UNS C26000 | ASTM B135 |
UNS C27000 | Tube, Pipe | UNS C27000 | ASTM B135 |
UNS C27450 | Tube | UNS C27450, EN CW509L, EN CuZn37 | ISO 1634 |
UNS C28000 | Tube | UNS C28000, EN CW509L, EN CuZn40 | ISO 1634 |
UNS C34500 | Rod | UNS C34500, BS CZ131, EN CW601N, EN CuZn35Pb2, BS CZ119, DIN 2.0331 | |
UNS C38000 | Rod | UNS C38000, BS CZ122, EN CW618N, JIS H3100, EN CuZn39Pb2 | ISO 1634 |
UNS C44300 | Tube | UNS C44300 | ASME SB111 |