Our core competencies mainly include semi-finished products and steel bars,Bright steel, tool steel, strip steel and sheet metal, wire, pipes, non-ferrous metal and Aluminum
Headquarters
Thalwil, Switzerland
Website
Type
Manufacturer and Processor
Grade | Shape | ||
---|---|---|---|
DIN St 37-2 | Bar | DIN St 37-2 | EN 10025, EN 10277-2 |
DIN St 52-3 | Bar | DIN St 52-3 | EN 10025, EN 10277-2 |
EN 1.4006 | Bar | EN 1.4006 | EN 10088-3 |
EN 1.4021 | Bar | EN 1.4021 | EN 10088-3 |
EN 1.4028 | Bar | EN 1.4028 | EN 10088-3 |
EN 1.4034 | Bar | EN 1.4034 | EN 10088-3 |
EN 1.4057 | Bar | EN 1.4057 | EN 10088-3 |
EN 1.4104 | Bar | EN 1.4104 | EN 10088-3 |
EN 1.4112 | Bar | EN 1.4112 | EN 10088-3 |
EN 1.4122 | Bar | EN 1.4122 | EN 10088-3 |