ISD Dunaferr

Claim this profile

About ISD Dunaferr

Hot rolled, pickled, cold rolled, galvanized strips and sheets, as well as open and hollow steel sections produced by ISD DUNAFERR are used primarily for the manufacturing of engineering, automotive and construction industrial products, as well as for the production of steel structures, household appliances and other parts.

Company profile

Headquarters

Dunaújváros, Hungary

Type

Manufacturer and Processor

Certifications

ISO 9001

, ISO 14001

, ISO 45001

, ISO 50001

Grades provided by the supplier

Grade Shape Equivalent Materials Standard / Norm 

API Gr A

Strip, Coil, Sheet, Plate

API Gr A

EN ISO 3183, API SPEC 5L

ASTM 1010

Strip, Coil, Sheet, Plate

ASTM 1010, SAE 1010

DIN 1614, ASTM A568

DASZ DHR 42

Strip, Coil, Sheet, Plate

DASZ DHR 42

DASZ 200

DASZ DN 1.0 Si

Strip, Coil, Sheet, Plate

DASZ DN 1.0 Si

DASZ 215

DIN EK2

Strip, Coil, Sheet, Plate

DIN EK2

DIN 1623, DASZ 206

DIN St 33

Strip, Coil, Sheet, Plate

DIN St 33

EN 10025-2, DIN 17100

DIN StW 22

Strip, Coil, Sheet, Plate

DIN StW 22

EN 10111, DIN 1614

DIN ZStE 260

Strip, Coil, Sheet, Plate

DIN ZStE 260

SEW 093

EN C22E

Strip, Coil, Sheet, Plate

EN C22E

EN 10083-2, EN 10083-3

EN P235GH

Strip, Coil, Sheet, Plate

EN P235GH

EN 10028-2, EN 10028-3, EN 10207, EN 10120

Showing 1 to 10 of 13 entries

Previous

1
2

Next