About Kaltband AG

As a manufacturer of demanding cold rolled products,Kaltband AG has found itself on the international market

Company profile

Headquarters

Reinach, Switzerland

Type

Manufacturer and Processor

Certifications

ISO 9001

Grades provided by the supplier

Grade Shape Equivalent Materials Standard / Norm 

EN 100Cr6

Strip

EN 100Cr6

EN 125Cr1

Strip

EN 125Cr1

EN 15Cr1

Strip

EN 15Cr1

EN 15Cr3

Strip

EN 15Cr3

EN 16MnCr5

Strip

EN 16MnCr5

EN 42CrMo4

Strip

EN 42CrMo4

EN 50CrMo4

Strip

EN 50CrMo4

EN 51CrV4

Strip

EN 51CrV4

EN 58CrV4

Strip

EN 58CrV4

EN 67SiCr5

Strip

EN 67SiCr5

Showing 1 to 10 of 21 entries